echnical Requirements For Clad Steel-Alu Explosive Transition Joint

 News     |      2019-10-26 09:07
1.Each batch must have ultrasonic inspection certificate.
2.Sampling inspection finished products 2 ~ 3%, fusion surface not less than 98%.
3. The tensile strength of contact surface shall not be less than 120MPa.
4.The shear strength of contact surface is not less than 80MPa.
5.Heat resisting not less than 400℃.
6. at room temperature 3000A current, voltage drop should not be higher than 2mv.
7. resistivity is less than 8.16× 10-8w ·m
8.The appearance is regular without any scar, and the welding seam shall not be cracked.
9.The thickness tolerance is 52±1, in which the aluminum plate is 12±1.
10.Material: aluminum 1070;For Q235B steel
 
 
 
As a new welding process, it can weld all kinds of metals with different strength, different expansion coefficient and different properties, saving precious metals, making it easy to combine and match the properties of lamination materials and base materials, widely used in electrolytic aluminum industry and metallurgy industry.
 
 
 